Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.40 g/cc
0.267 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 15
15
Tensile Strength at Break 48.00 MPa
6962 psi
Elongation at Break 36.5 %
36.5 %
Shear Strength 27.00 MPa
3916 psi
Thermal Properties Metric English Comments
Melting Point 217 °C
423 °F
Eutectic
Solidus 217 °C
423 °F
Eutectic
Liquidus 217 °C
423 °F
Eutectic
Component Elements Properties Metric English Comments
Copper, Cu 0.70 %
0.70 %
Silver, Ag 3.8 %
3.8 %
Tin, Sn 95.5 %
95.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000130 ohm-cm
0.0000130 ohm-cm