Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 220 Silver Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 220 Silver Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.01 g/cc
0.3616 lb/in³
Thermal Properties Metric English Comments
Melting Point 775 - 785 °C
1430 - 1450 °F
Solidus 775 °C
1430 °F
Liquidus 785 °C
1450 °F
Component Elements Properties Metric English Comments
Copper, Cu 28 %
28 %
Nickel, Ni 0.50 %
0.50 %
Silver, Ag 71.5 %
71.5 %
Users viewing this material also viewed the following: