C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated to multiple tempers -- are available in a choice of strength, hardness and thermal conductivity levels.C17510 Beryllium Copper is manufactured to provide a good strength with even better thermal conductivity than C17200. This copper alloy offers conductivity of 45 to 60 percent of pure copper while providing significant strength and hardness properties. This copper alloy is often used in the resistance welding industry.Information provided by IBC Advanced Alloys.
Physical Properties Metric English Comments
Density 8.83 g/cc
0.319 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 92 - 100
92 - 100
Tensile Strength 689 - 896 MPa
100000 - 130000 psi
Tensile Strength, Yield 552 - 689 MPa

@Strain 0.200 %
80000 - 100000 psi

@Strain 0.200 %
Elongation at Break >= 10 %
>= 10 %
Modulus of Elasticity 138 GPa
20000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.6 µm/m-°C
9.80 µin/in-°F
Thermal Conductivity 242 W/m-K
1680 BTU-in/hr-ft²-°F
Melting Point 1040 - 1080 °C
1900 - 1980 °F
Solidus 1040 °C
1900 °F
Liquidus 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.20 - 0.60 %
0.20 - 0.60 %
Copper, Cu 97.2 - 98.4 %
97.2 - 98.4 %
As Balance
Nickel, Ni 1.4 - 2.2 %
1.4 - 2.2 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.00000380 ohm-cm
<= 0.00000380 ohm-cm