Hong Kun Group Aluminum-N-nitroso-N-phenylhydroxyamine Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hong Kun Group Aluminum-N-nitroso-N-phenylhydroxyamine Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CAS No. 15305-07-4All information provided by Hongkun Group
Physical Properties Metric English Comments
Molecular Weight 438.33 g/mol
438.33 g/mol
Thermal Properties Metric English Comments
Melting Point 160 - 172 °C
320 - 342 °F
Descriptive Properties Value Comments
Appearance off white to yellow powder
Purity (%) > 98
HPLC