Material Notes:
Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Extremely hard and wear resistant to meet the more demanding requirements of electrical upsetting and electro-forging.Data provided by Hogen Industries.
Physical Properties Metric English Comments
Density >= 12.3 g/cc
>= 0.444 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32
32
Tensile Strength, Ultimate 586 MPa
85000 psi
Thermal Properties Metric English Comments
CTE, linear 9.80 µm/m-°C

@Temperature 20.0 °C
5.44 µin/in-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Copper, Cu 30 %
30 %
WC 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000570 ohm-cm
0.00000570 ohm-cm