Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexForce™ 4526 Fiber Glass Fabric

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ 4526 Fiber Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential allowing the end user to choose the best combination for material performance, economics and product flexibility.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 152 microns
6.00 mil
Mechanical Properties Metric English Comments
Tensile Impact 187 J/cm
350 ft-lb/in
Warp Breaking Strength
187 J/cm
350 ft-lb/in
Filling Breaking Strength
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 5.6
Dry
Nominal Construction (count/in) 34
Fill
36
Warp
Type of Yarn Fill Yarn: SCG 75 1/0 493
Warp Yarn: SCG 75 1/0 493
Weave Style 2x2 Basket