ROVENE® 9410 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion. Its relative high molecular weight and styrene content (25%) permits the formulation of pressure sensitive adhesives with a wide variety of tackifiers. With its unique balance of molecular weight and styrene content, it is an ideal candidate for blending with natural rubber and formulation of low temperature adhesives.APPLICATIONS: ROVENE® 9410 is recommended for pressure sensitive permanent label adhesives for low temperature applications and blended with natural latex for high shear tape adhesives.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 49 - 51.5 %
49 - 51.5 %
Particle Size 0.16 µm
0.16 µm
pH 8.5 - 9.0
8.5 - 9.0
Brookfield Viscosity 600 cP
600 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -56.0 °C
-68.8 °F
Chemical Properties Metric English Comments
Styrene Content 25 %
25 %
Descriptive Properties Value Comments
Emulsifiers Anionic