Fainplast Compounds Hax™ HFC 0115/1 Flame Retardant Polyolefin Cable Compound

Category Polymer , Thermoplastic , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer Fainplast Compounds
Trade Name Hax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds Hax™ HFC 0115/1 Flame Retardant Polyolefin Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds
Physical Properties Metric English Comments
Density 1.88 - 1.92 g/cc
0.0679 - 0.0694 lb/in³
ISO 1183
Melt Flow 82 - 92 g/10 min

@Load 21.6 kg,
Temperature 150 °C
82 - 92 g/10 min

@Load 47.6 lb,
Temperature 302 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 28 - 34
28 - 34
ISO 868
Thermal Properties Metric English Comments
Oxygen Index 52 - 58 %
52 - 58 %
ISO 4589
Processing Properties Metric English Comments
Processing Temperature 100 - 180 °C
212 - 356 °F
extruder
Shelf Life 3.00 Month

@Temperature 30.0 °C
3.00 Month

@Temperature 86.0 °F
Moisture absorption after extended storage