Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Heatbath/Park AL-2 for Aluminum Solution Heat Treating

Category Ceramic , Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park AL-2 for Aluminum Solution Heat Treating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A granular mixture of sodium and potassium nitrates formulated per MIL-H-6088. It is less costly than Tempering C-ALHT with only a slight sacrifice in working range. It is colored pink for identification purposes.Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Maximum Service Temperature, Air 593 °C
1100 °F
Upper limit of working range
Minimum Service Temperature, Air 288 °C
550 °F
Lower limit of working range