HOME
ABOUT US
PRODUCT
Thermoplastic
Thermoset
Adhesive
RenewableRecycled-Polymer
RenewableRecycled-Film
Tape
RECENT UPDATE
Company News
Product News
CONTACT US
RFQ
POLYMER SEARCH
SEARCH
HOME
POLYMER SEARCH
Haynes International, Inc.
Manufacturer :
Haynes International, Inc.
Product List
Category
Cobalt Alloy
Superalloy
Nickel Alloy
Iron Base
Alpha/Near Alpha Titanium Alloy
Trade Name
Hastelloy®
Multimet®
Ultimet®
Tips:
Up to 100 items are displayed.
PRODUCT NO.
Category
Trade Name
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Superalloy
Haynes 188 alloy, plate at RT after 8000 hours at 870°C (1600°F)
Superalloy
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes
Superalloy
Haynes 230® alloy, plate, 4000 hours exposure at 760°C (1400°F)
Superalloy
Haynes 25 alloy, cold worked sheet, 15% cold reduction, aged at 370°C (700°F) for 1 hour
Superalloy
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours
Superalloy
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F)
Superalloy
Hastelloy®
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F)
Superalloy
Hastelloy®
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 4000 hours
Superalloy
Hastelloy®
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours
Superalloy
Hastelloy®
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments
Superalloy
Hastelloy®
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Iron Base
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Iron Base
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F)
Superalloy
Haynes HR-160® alloy, solution annealed sheet
Superalloy
Haynes Multimet® alloy, 12.7 mm (1/2 in.) thick plate, 1185°C heat treatment, water quenched
Iron Base
Multimet®
Haynes Multimet® alloy, 25.4-50.8 mm forged bar, 1185°C heat treatment, water quenched
Iron Base
Multimet®
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Superalloy
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Superalloy
Ultimet®
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Superalloy
Ultimet®
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Superalloy
Ultimet®
Haynes Waspaloyâ„¢ alloy, sheet
Superalloy
Haynes 25 alloy, room temperature after 25% cold reduction
Superalloy
Haynes 25 alloy, room temperature after 25% cold reduction, 1175°C anneal for 5 minutes
Superalloy
Haynes 25 alloy, room temperature sheet after 100 hours of 760°C exposure
Superalloy
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Nickel Alloy
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel Alloy
Haynes 556® alloy, 0% cold reduction, 1065°C anneal for 5 minutes
Iron Base
Haynes 556® alloy, 30% cold reduction
Iron Base
Haynes 556® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
Iron Base
Haynes 556® alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick
Iron Base
Haynes 625 alloy, plate after 1000 hours at 870°C (1600°F)
Superalloy
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
Superalloy
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc
Superalloy
Hastelloy®
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate
Superalloy
Hastelloy®
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel Alloy
Hastelloy®
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Nickel Alloy
Hastelloy®
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Superalloy
Hastelloy®
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F)
Superalloy
Haynes 25 alloy, room temperature after 10% cold reduction, 1175°C anneal for 5 minutes
Superalloy
Haynes 556® alloy, 20% cold reduction, 1010°C anneal for 5 minutes
Iron Base
Haynes 556® alloy, bar after 16000 hours at 760°C (1400°F)
Iron Base
Haynes 625 alloy, 30% cold reduction, 1010°C anneal for 5 minutes
Superalloy
Haynes Hastelloy® alloy 625 12.7 mm plate weldments
Superalloy
Hastelloy®
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Nickel Alloy
Hastelloy®
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C
Superalloy
Hastelloy®
Haynes Hastelloy® G-30® alloy, 10% cold rolled
Superalloy
Hastelloy®
Haynes 230® alloy, 50% cold reduction, 1121°C anneal for 5 minutes
Superalloy
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel Alloy
Hastelloy®
HOME
ABOUT US
POLYMER SEARCH
COMPANY NEWS
PRODUCT NEWS
CONTACT US
RFQ
Copyright © lookpolymers.com All Rights Reserved