Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

H.C. Starck Molybdenum Alloy AFB, Arc-Cast Forging Billet

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal , Pure Element
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Molybdenum Alloy AFB, Arc-Cast Forging Billet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This specification covers carbon-deoxidized molybdenum wrought forging billets produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting process.Structure: The billets will be supplied in the recrystallized condition, with a maximum hardness of 200 B.H.N. (10 mm ball/1500 kg/30 sec.). Material can also be supplied in the stress-relieved condition.Information provided by H.C. Starck.
Mechanical Properties Metric English Comments
Hardness, Brinell <= 200

@Load 1500 kg,
Time 30.0 sec
<= 200

@Load 3310 lb,
Time 0.00833 hour
10 mm ball
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Iron, Fe <= 0.0080 %
<= 0.0080 %
Molybdenum, Mo >= 99.95 %
>= 99.95 %
by difference
Nickel, Ni <= 0.0020 %
<= 0.0020 %
Nitrogen, N <= 0.0020 %
<= 0.0020 %
Oxygen, O <= 0.0015 %
<= 0.0015 %
Silicon, Si <= 0.0080 %
<= 0.0080 %
Users viewing this material also viewed the following: