Hexcel® HexForce™ 220HT Fiber Glass Fabric

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ 220HT Fiber Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential allowing the end user to choose the best combination for material performance, economics and product flexibility.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 88.9 microns
3.50 mil
Mechanical Properties Metric English Comments
Tensile Impact 144 J/cm
270 ft-lb/in
Filling Breaking Strength
147 J/cm
275 ft-lb/in
Warp Breaking Strength
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 3.06
Dry
Nominal Construction (count/in) 58
Fill
60
Warp
Type of Yarn Fill Yarn: SCE 225 1/0 933
Warp Yarn: SCE 225 1/0 933
Weave Style 4 Harness Satin