Gwent Electronic Materials C2100211D1 Silicone Based Silver Paste

Category Fluid , Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2100211D1 Silicone Based Silver Paste.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This ink can be used in a wide range of applications, as conductive adhesive, it has excellent chemical resistance, with good adhesion. This product has been tested at 250°C and it showed good stability for minimum 12 weeks. Screen Printing Equipment: semi-automatic, automaticScreen Types: stainless steel, polyesterSubstrate: Ceramic or metallic substrateInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Storage Temperature 20.0 °C
68.0 °F
sealed container
Component Elements Properties Metric English Comments
Silver, Ag 69 - 71 %
69 - 71 %
Theoretical
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.040 ohm

@Temperature 200 °C
0.040 ohm

@Temperature 392 °F
Cured Film at 200°C for 30 min
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 60.0 °C
0.250 hour

@Temperature 140 °F
first step
30.0 min

@Temperature 200 °C
0.500 hour

@Temperature 392 °F
second step
Shelf Life 6.00 Month
6.00 Month