Carbon conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and good conductivity.Testing was carried out on a Timsons T-Flex 508 and Nilpeter FB-3300.Substrate: Polyester, PVC, BOPP, Cellophane, Paper or Cellulosic Board.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 30 - 34 %

@Temperature 130 °C
30 - 34 %

@Temperature 266 °F
Viscosity 200 - 500 cP

@Shear Rate 50.0 1/s,
Temperature 25.0 °C
200 - 500 cP

@Shear Rate 50.0 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Volume Resistivity 0.0109 ohm-cm
0.0109 ohm-cm
Printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
Surface Resistivity per Square 350 - 400 ohm

@Thickness 0.0250 mm
350 - 400 ohm

@Thickness 0.000984 in
Printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
1400 - 1600 ohm

@Thickness 0.00500 mm
1400 - 1600 ohm

@Thickness 0.000197 in
Printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
Users viewing this material also viewed the following: