Gwent Electronic Materials C2071218D1 Gold Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2071218D1 Gold Ink.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Gold Ink C2071218D1 is a fritted system that has been designed as a screen printing termination ink NTC components. It is also suitable for firing onto other high temperature substrates.This product is RoHS compliant.This product is suitable for repeat firing application where minimal change in electrical conductivity is required. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 230-325 tpiSubstrate: NTC components, alumina and other high temperature substratesInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 79 - 81 %

@Temperature 700 °C
79 - 81 %

@Temperature 1290 °F
Viscosity 4500 - 7500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
4500 - 7500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Sintering Temperature 750 - 850 °C
1380 - 1560 °F
Cure Time 10.0 min

@Temperature 125 °C
0.167 hour

@Temperature 257 °F
15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 91
Using a 230 mesh stainless steel screen