Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed CHEMRAZ® 565 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Greene Tweed CHEMRAZ® 565 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE. Chemraz designs last longer and seal better in harsh environments at a wider range of temperatures than any other elastomer on the market. Chemraz solves some of the most difficult sealing problems encountered in many industries while delivering outstanding in-use cost effectiveness through custom components.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.93 g/cc
1.93 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength at Break 12.1 MPa
1750 psi
ASTM D1414
Tensile Strength, Yield 3.10 MPa
450 psi
@50% Elongation; ASTM D1414
7.93 MPa
1150 psi
@100% Elongation; ASTM D1414
Elongation at Break 140 %
140 %
ASTM D1414
Compression Set 25 %
25 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
26 %
26 %
1000 hours @ 300°F(4 more Hr. PC @ 300°F) @ 25% deflection; ASTM D395
41 %
41 %
1000 hours @ 300°F @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: