Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed Arlon® 1260 Polyketone, Carbon Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Greene Tweed
Trade Name Arlon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Arlon® 1260 Polyketone, Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Arlon® 1260 is a carbon-fiber reinforced version of Arlon 1000 featuring the highest modulus and tensile strength of all the Arlon grades. Designers requiring a low coefficient off thermal expansion often select Arlon 1260.Arlon 1260 also provides enhanced Tribological properties, reduced friction values and improved wear properties over Arlon 1000. Arlon 1260 is ideal in lubricated bearings and/or moist environments.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 92
92
ASTM D2240
Tensile Strength at Break 230 MPa
33400 psi
ASTM D368
Elongation at Break 1.9 %
1.9 %
ASTM D638
Tensile Modulus 21.7 GPa
3150 ksi
ASTM D638
Flexural Strength 347 MPa
50300 psi
ASTM D790
Flexural Modulus 19.0 GPa
2750 ksi
ASTM D790
Compressive Strength 262 MPa
38000 psi
ASTM D695
Descriptive Properties Value Comments
Color Black