Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
15 sec; ASTM D2240
Tensile Strength at Break 20.9 MPa
3030 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 15.9 MPa

@Strain 100 %
2310 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 280 %
280 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 105 kN/m
599 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -16.1 °C
3.02 °F
ASTM D746
Oxygen Index 26 %

@Thickness 3.18 mm
26 %

@Thickness 0.125 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 179 - 185 °C
354 - 365 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Features Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Profile Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Furniture