Material Notes:
GRAFOIL® Grade GHW is a laminate made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0025" thick high-temperature continuous woven glass fiber insert. Its functional temperature range is -240°C to 400°C (-400°F to 750°F). Grade GHW is a patented product (US Patent 4,961,991) with excellent strength and handling characteristics. In addition, GHW laminates have excellent blowout resistance and high-temperature creep relaxation characteristics when compared to good quality asbestos, aramid, and carbon fiber gasket materials. GHW is fire safe, and elevated temperature testing proves that GHW outperformed asbestos gasket materials. Its applications include valves, pumps, pipe/ASME/API/DIN flanges, glass-lined or low load flange equipment, steam traps, heat exchangers, and compressors. The advantages of grade GHW are compatible with a wide range of chemicals; maximum continuous use temperature 400°C (750°F); no shelf life; material availability in rolls allows for maximum material utilization; cost effective; easily cut; contains no hazardous materials; robust enough for easy handling and durability; superior to non-asbestos fiber sheet in every characteristic (Temp, Creep, Recovery, and Sealability). Laminate Construction: GRAFOIL® Grade GTB ? 0.0025" high-temperature, PTFE impregnated, continuous woven glass fiber insert ? GRAFOIL® Grade GTB. The Max Operating Pressure is rated for ASME class 150 or class 300 flanges.
Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
Thickness 1570 microns
61.8 mil
Standard
3100 microns
122 mil
Standard
Mechanical Properties Metric English Comments
Compression Set 85 %

@Pressure 34.5 MPa
85 %

@Pressure 5000 psi
after 5000 psi load
Descriptive Properties Value Comments
"m" Factor 2
ASME Gasket Factor
"y" Stress (psi) 900
ASME Gasket Factor
Compressibility (%) 40
at 5000 psi load
Max Gasket Unit Load (psi) 24000
ASME Gasket Factor