Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global GP-5180-30 PET 30% Glass Reinforced PET Polyester  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GP-5180-30 PET 30% Glass Reinforced PET Polyester  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 170 MPa
24700 psi
5 mm/min; ISO 527-2/1A
Elongation at Break 2.6 %
2.6 %
5 mm/min; ISO 527-2/1A
Flexural Yield Strength 270 MPa
39200 psi
ISO 178
Flexural Modulus 11.0 GPa
1600 ksi
ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
ISO 180/1A
Users viewing this material also viewed the following: