Material Notes:
Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregular surfacesEasy to cut and handle, extremely flexibleCertified NSF 61 material (drinking water)Information provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0492 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 6.89 MPa
1000 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C

@Pressure 3.45 MPa
400 °F

@Pressure 500 psi
Continuous
Minimum Service Temperature, Air -73.3 °C
-100 °F
Descriptive Properties Value Comments
Color Blue/Off-White
Compressibility, % 15-30
ASTM F36
Creep Relaxation, % 30
ASTM F38
Sealability ASTM F37B, ml/hr 0.15
ASTM Fuel A
0.2
Nitrogen