Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills P5M6K-101X Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5M6K-101X Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Excellent clarity and processing. Product does not contain animal derived components. Phthalate-freeApplications: Injection molding - high clarity parts and medical devicesInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 28.6 MPa
4150 psi
ASTM D638
Elongation at Yield 11.5 %
11.5 %
ASTM D638
Flexural Modulus 1.04 GPa
151 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.630 J/cm
1.18 ft-lb/in
ASTM D256
Gardner Impact 36.2 J
26.7 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1a
Users viewing this material also viewed the following: