Fibre Glast 530 Plain Weave Carbon Fiber Fabric

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 530 Plain Weave Carbon Fiber Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Graphite fibers contain up to 95% carbon and yield the highest tensile strength in the FRP industry. These fibers woven together form graphite fabric. These fabrics offer higher strength and stiffness-to-weight ratios than any other commonly available reinforcements. While there are hundreds of types to choose from, we have selected three styles of standard modulus carbon fiber which are suitable for use in racing, aircraft, competition marine, and light industrial applications. To maximize the fiber properties we recommend using only epoxy or vinyl ester resin, although polyesters will bond to the fabrics. This plain weave carbon fiber is the most commonly used type for lightweight aerodynamic parts.General Properties for Carbon Fiber Fabrics: Lightweight; High Modulus; High Strength; Fire Resistant; Dimensionally Stable; Fatigue Resistant
Physical Properties Metric English Comments
Thickness 305 microns
12.0 mil
Descriptive Properties Value Comments
Weight (oz/sq yd) 5.7
Yarn Description, Fill 3K Multifilament Cont. Tow
Yarn Description, Warp 3K Multifilament Cont. Tow