Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds RI 52 Rigid PVC, Injection Molding

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Fainplast Compounds RI 52 Rigid PVC, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fittings for building trade
Physical Properties Metric English Comments
Density 1.42 - 1.46 g/cc
0.0513 - 0.0527 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ISO R 527
Tensile Strength, Yield 42.0 MPa
6090 psi
ISO R527
Elongation at Break 100 %
100 %
ISO R 527
Izod Impact, Unnotched 0.400 - 0.800 J/cm

@Temperature 23.0 °C
0.749 - 1.50 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 80.0 - 82.0 °C

@Load 5.00 kg
176 - 180 °F

@Load 11.0 lb
ISO R306
Users viewing this material also viewed the following: