| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade | 
| Manufacturer | Fainplast Compounds | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Fainplast Compounds HL 92/1 Flexible PVC, Insulation for High Temperatures.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | 90 - 94 | 90 - 94 | ISO R 868 | 
| Tensile Strength at Break | >= 19.0 MPa | >= 2760 psi | ISO R 527 | 
| Elongation at Break | >= 320 % | >= 320 % | ISO R 527 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Oxygen Index | 28 % | 28 % | ISO 4589 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity |           1.50e+14           ohm-cm           @Temperature 23.0 °C  | 
                  1.50e+14           ohm-cm           @Temperature 73.4 °F  | 
        ASTM D257 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Thermal Stability (minutes) | 180 | CEI 20-34/3-2 |