Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.50 - 1.54 g/cc
0.0542 - 0.0556 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 89
85 - 89
ISO R 868
Tensile Strength at Break >= 14.0 MPa
>= 2030 psi
ISO R 527
Elongation at Break >= 210 %
>= 210 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -22.0 °C
-7.60 °F
Cold Flex; ISO 458/2
Descriptive Properties Value Comments
Thermal Stability (minutes) 100
CEI 20-34/3-2