Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CIMBAR CIMBAR™ CF Barite Powder (BaSO4)

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name CIMBAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR CIMBAR™ CF Barite Powder (BaSO4).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical inertness make then ideal for many applications.Uses:Coatings: Automotive Primers, Automotive Topcoats, High Gloss Enamel, Powder Coatings, Semi-gloss Latexes, Gloss Latexes, Industrial Coatings, Architectural Coatings, Maintenance Coatings, Industrial PrimersFillers: Plastics, Ceramics, Friction Materials, Rubber Goods, Plastisols, Adhesives, Latex Products, Urethane Foams, Acoustical Compounds, Insulating Materials, Sound Attenuation ProductsInformation provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 4.40 g/cc
4.40 g/cc
Brightness 93 %
93 %
"L"
Oil Absorption 10 %
10 %
Fineness 5.5
5.5
Hegman Fineness
Apparent Bulk Density 1.12 g/cc
0.0405 lb/in³
Loose
1.84 g/cc
0.0666 lb/in³
Compacted
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Loss On Ignition 0.75 %
0.75 %
Particle Size 4.5 µm
4.5 µm
Median
<= 20 µm
<= 20 µm
Max
Particle Mesh Size 325 Mesh
325 Mesh
0.0% retained
pH 8.5
8.5
Component Elements Properties Metric English Comments
Al2O3 0.010 %
0.010 %
Fe2O3 0.020 %
0.020 %
Trace Metals 0.050 %
0.050 %
Heavy Metals
Descriptive Properties Value Comments
BaSO4 (%) 98
Total Silicates (%) 0.82
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved