ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult injection molding applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Non-hygroscopic product, requires little to no drying before processing.Neutral, easy coloring formulation.Excellent sealing properties.DishwasherabilityInformation provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 21
21
Air at 158°F, 168 hr; ASTM D573
23

@Thickness 2.00 mm
23

@Thickness 0.0787 in
ISO 868
Tensile Strength at Break 2.184 MPa
316.8 psi
Air at 158°F, 168 hr; ASTM D573
2.21 MPa
320 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 0.483 MPa
70.0 psi
Across Flow; ASTM D412
Elongation at Break 350 %
350 %
Across Flow; ASTM D412
423.5 %
423.5 %
Air at 158°F, 168 hr; ASTM D573
Compression Set 11 %
11 %
73°F, 22 hr; ASTM D395
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets