Material Notes:
A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner molding, end caps and special fixation applications, and for COF enhancement. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Key Features:Specially formulated to replace thermoset EPDM rubber in automotive glass run channel corner molding applications.Designed for shorter processing time compared to thermoset EPDM rubber.Adheres to vulcanized EPDM rubber over wide range of temperatures.Adheres to TPV over wide range of temperatures.Enhanced COF properties.Good UV resistance.Low fogging.Paint stain resistant.Applications:Automotive- Weather SealsUses:Automotive ApplicationsAutomotive Exterior Trim Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
2 mm, 15 sec; ISO 868
Tensile Strength at Break 6.00 MPa
870 psi
Across Flow; ASTM D412
Tensile Stress 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 470 %
470 %
Across Flow; ASTM D412
Compression Set 44 %
44 %
158°F, 22 hr; ASTM D395
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 54
Color Black
Form Pellets
Copyright © lookpolymers.com All Rights Reserved