Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil HDPE HPA 020 Molding High Density Polyethylene (HMW) Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil HDPE HPA 020 Molding High Density Polyethylene (HMW) Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: HPA 020 is a high molecular weight HDPE resin, characterized by excellent balance of rigidity, ESCR and impact strength. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: Yes Applications: Drainage PipesHeavy Gauge SheetLarge Part Blow MoldingLarge Parts & Containers (20 to 100 L) for non-food end usesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D4883
ESCR 100% Igepal® 600 hour
600 hour
ASTM D1963
ESCR 10% Igepal® 490 hour
490 hour
ASTM D1963
Melt Flow 9.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63

@Time 15.0 sec
63

@Time 0.00417 hour
ASTM D2240
Tensile Stress 15.2 MPa

@Strain 100 %
2200 psi

@Strain 100 %
2 in/min; ASTM D412
Tensile Strength, Yield 24.8 MPa
3600 psi
2 in/min; ASTM D638
Elongation at Break >= 100 %
>= 100 %
2 in/min; ASTM D638
Tensile Modulus 0.965 GPa
140 ksi
2 in/min; ASTM D638
Izod Impact, Notched 0.379 J/cm
0.710 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Users viewing this material also viewed the following: