Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Esstech X-969-0000 Ethoxyethyl Methacrylate, C8H14O3

Category Polymer , Thermoset , Methacrylate
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-969-0000 Ethoxyethyl Methacrylate, C8H14O3.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EOEMA is a high purity methacrylate monomer often used for, but not limited to contact lens applications. Listed on the Toxic Substance Control Act List. CAS # 51289-08-8.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
Molecular Weight 158.2 g/mol
158.2 g/mol
Optical Properties Metric English Comments
Refractive Index 1.4275
1.4275
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Acidity (% Methacrylic Acid) < 0.05
Color (APHA) < 25
MeHQ Inhibitor (ppm) 50-300
Purity (%) > 95