| Category | Polymer , Thermoset , Epoxy , Epoxy, High Temperature |
| Manufacturer | Epoxy Technology |
| Trade Name | EPO-TEK® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.990 g/cc | 0.990 g/cc | Part B |
| 1.20 g/cc | 1.20 g/cc | Part A | |
| Particle Size | <= 20 µm | <= 20 µm | |
| Viscosity | 3500 - 6000 cP @Temperature 23.0 °C |
3500 - 6000 cP @Temperature 73.4 °F |
50 rpm |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 88 | 88 | |
| Tensile Modulus | 2.54 GPa | 369 ksi | Storage |
| Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
| >= 46.9 MPa | >= 6800 psi | Die |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 34.0 µm/m-°C | 18.9 µin/in-°F | Below Tg |
| 129 µm/m-°C | 71.7 µin/in-°F | Above Tg | |
| Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
| 350 °C | 662 °F | Intermittent | |
| Minimum Service Temperature, Air | -55.0 °C | -67.0 °F | Continuous |
| -55.0 °C | -67.0 °F | Intermittent | |
| Glass Transition Temp, Tg | >= 100 °C | >= 212 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
| Decomposition Temperature | 415 °C | 779 °F | Degradation Temperature |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.5715 @Wavelength 589 nm |
1.5715 @Wavelength 589 nm |
|
| Transmission, Visible | >= 90 % @Wavelength 520 - 1660 nm |
>= 90 % @Wavelength 520 - 1660 nm |
Spectral |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 3.00e+13 ohm-cm | >= 3.00e+13 ohm-cm | |
| Dielectric Constant | 2.58 @Frequency 1000 Hz |
2.58 @Frequency 1000 Hz |
|
| Dissipation Factor | 0.0080 @Frequency 1000 Hz |
0.0080 @Frequency 1000 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 30.0 min @Temperature 90.0 °C |
0.500 hour @Temperature 194 °F |
minimum |
| Pot Life | 480 min | 480 min | |
| Shelf Life | 12.0 Month @Temperature 25.0 °C |
12.0 Month @Temperature 77.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Clear | Part A |
| Slightly Yellow | Part B | |
| Consistency | Pourable liquid | |
| Mix Ratio By Weight | 10:1 | |
| Number of Components | Two | |
| Weight Loss | 0.28% | 200°C |
| 0.42% | 250°C | |
| 0.86% | 300°C |