Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mid-Mountain Materials THERMOSEAL® A Rigidizer

Category Fluid
Manufacturer Mid-Mountain Materials
Trade Name THERMOSEAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials THERMOSEAL® A Rigidizer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Thermoseal® Rigidizers are low viscosity liquids which, when applied to the surface of ceramic fiber and other permeable products, impart surface hardness and improve resistance to erosion. APPLICATION: THERMOSEAL® RIGIDIZERS are applied by brush, roller, spray or by dipping. Multiple applications, with drying between each application, will increase surface hardness. THERMOSEAL® RIGIDIZERS are relatively non-toxic, however, excessive or prolonged inhalation of mists or dust resulting from their application should be avoided. These compounds should not be allowed to freeze repeatedly.DRYING: THERMOSEAL® RIGIDIZERS may be air dried or force-dried by heating with flame or in an oven. A slow bake-out at approximately 200ºF • 95ºC is most desirable for Rigidizer S and 300-400ºF • 150-205ºC for Rigidizer A.PACKAGING: THERMOSEAL® RIGIDIZERS are available in one gallon and five gallon buckets.Information provided by Mid-Mountain Materials.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Solids Content 20 %
20 %
pH 4.0
4.0
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1370 °C
2500 °F
Use Limit
Descriptive Properties Value Comments
Color White opalescent
Users viewing this material also viewed the following: