UCAR Carbon UCAR® ATA Isostatic Molded Graphite

Category Carbon , Graphite
Manufacturer UCAR Carbon Company (GrafTech International)
Trade Name UCAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UCAR Carbon UCAR® ATA Isostatic Molded Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Economical grade ATA is the lowest density version of isostatically molded, fine grain grade ATJ family of graphite materials.Typical Applications: ATA is used in general purpose applications where a fine grain structure and surface finish are needed such as mandrels and molds.Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
Particle Size 25 µm
25 µm
Ash 0.090 %
0.090 %
Mechanical Properties Metric English Comments
Flexural Strength 20.7 MPa
3000 psi
Thermal Properties Metric English Comments
CTE, linear 2.80 µm/m-°C

@Temperature 20.0 - 100 °C
1.56 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 90.0 W/m-K
625 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00130 ohm-cm
0.00130 ohm-cm