Covestro Texin® DP 7-1158 Urethane Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Texin® DP 7-1158 Urethane Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Suitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.00 MPa
1020 psi
Stress at 50% Strain
Elongation at Break >= 50 %
>= 50 %