Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eagle Brass 18665 MSP1, Extra Hard

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Eagle Brass Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 18665 MSP1, Extra Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs, switches, sockets, and junction boxes.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.94 g/cc
0.323 lb/in³
Annealed
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 538 - 627 MPa
78000 - 91000 psi
Tensile Strength, Yield 490 - 621 MPa
71000 - 90000 psi
0.2% offset
Elongation at Break >= 5.0 %
>= 5.0 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.3 µm/m-°C

@Temperature 20.0 - 300 °C
9.60 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 456.5 W/m-K
3168 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 99 %
99 %
Magnesium, Mg 0.70 %
0.70 %
Phosphorous, P 0.040 %
0.040 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000283 ohm-cm
0.00000283 ohm-cm
Annealed
Users viewing this material also viewed the following: