Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ELASTO UK Dryflex® 662750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Black

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 662750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine the advantages of the other two series. The material has good flow and mechanical properties as well as reasonable scratch resistance.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75

@Thickness 4.00 mm
75

@Thickness 0.157 in
ASTM D2240
Tensile Strength at Break 9.00 MPa
1310 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
100% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
Tear Strength 33.0 kN/m
188 pli
ASTM D624
Compression Set 25 %
25 %
at 23°C, 72 hrs; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Processing Properties Metric English Comments
Processing Temperature 180 - 210 °C
356 - 410 °F
Descriptive Properties Value Comments
Bonding to PP Excellent
Chemical Resistance Good
Excluding organic solvents, aromatic and vegetable oils
Color Black
Weather Resistance Excellent
Air ageing