E-Polymers EFLEX® S3160 Overmolding

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE , Polypropylene (PP)
Manufacturer E-Polymers Co. Ltd.
Trade Name EFLEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers EFLEX® S3160 Overmolding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplastic equipment. Overmolding grade is based on SEBS/SEEPS/engineering plastics and exhibit excellent adhesion to engineering plastics as PA, PC, ABS, PC/ABS, PBT. It has product lines for general grade, transparent grade, overmolding grade, high temperature grade, medical grade and extrusion grade.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
ASTM D2240
Tensile Strength 10.01 MPa
1451 psi
ASTM D412
Elongation at Break 670 %
670 %
ASTM D412
Descriptive Properties Value Comments
Adhesion to Plastic 5.5-5.9 kg/in