DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® 473 is a high clarity polyester film manufactured with a coating on one surface that improves slip and handling characteristics. The opposite surface is raw polyester (non-coated). The slip treated surface is wound inside of the roll and the raw surface (non-coated) is on the outside surface of the roll.Typical Applications: Melinex 473 is used in many general industrial applications where clarity and handling properties are critical, e.g., overlay, lamination and printing applications.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 89.6 MPa
>= 13000 psi
ASTM D882A
Film Tensile Strength at Yield, TD >= 89.6 MPa
>= 13000 psi
ASTM D882A
Coefficient of Friction, Dynamic <= 0.70
<= 0.70
A-B; ASTM D1894
Film Tensile Strength at Break, MD >= 172 MPa
>= 25000 psi
ASTM D882A
Film Tensile Strength at Break, TD >= 172 MPa
>= 25000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 9918 in2/lb