Material Notes:
DuPont™ Fusabond® E158H is a anhydride modified polyethylene. Uses: Adhesives Coating Applications Pipe Coating Tie-Layer
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D792, ISO 1183
Melt Flow 1.65 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.65 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Adhesive Bond Strength 11.33 MPa
1644 psi
Lap Shear; ASTM D1002
Thermal Properties Metric English Comments
Melting Point 113 °C
235 °F
Freezing Point; ASTM D3418
128 °C
262 °F
ASTM D3418, ISO 3146
Vicat Softening Point 102 °C
216 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 290 °C
<= 554 °F