| Category | Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC |
| Manufacturer | PolyOne Corporation |
| Trade Name | Elastamax™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Elastamax™ HTE 1105 Styrene Butadiene Block Copolymer (SBC).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.938 g/cc | 0.938 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 40 | 40 | ASTM D2240 |
| Tensile Strength at Break | 8.89 MPa | 1290 psi | 510 mm/min; ASTM D412A |
| Tensile Stress | 1.59 MPa @Strain 100 % |
231 psi @Strain 100 % |
510 mm/min; ASTM D412A |
| 2.28 MPa @Strain 300 % |
331 psi @Strain 300 % |
510 mm/min; ASTM D412A | |
| Elongation at Break | 1100 % | 1100 % | 510 mm/min; ASTM D412A |
| Tear Strength | 29.8 kN/m | 170 pli | Die C, 510 mm/min; ASTM D624 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | General Purpose | |
| Forms | Pellets | |
| Generic Material | SBC | |
| Generic Name | Styrene Butadiene Block Copolymer (SBC) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Automotive Interior Parts | |
| Consumer Applications | ||
| General Purpose | ||
| Industrial Applications |