| Category | Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Dow Corning SE 4486 SILICONE RTV.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.59 g/cc <br>@Temperature 25.0 °C |
2.59 g/cc <br>@Temperature 77.0 °F |
|
| Viscosity | 19000 cP | 19000 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 78 | 78 | |
| Tensile Strength, Ultimate | 3.80 MPa | 551 psi | |
| Elongation at Break | 50 % | 50 % | |
| Shear Strength | 1.38 MPa | 200 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 124 µm/m-°C | 68.9 µin/in-°F | |
| Thermal Conductivity | 1.53 W/m-K | 10.6 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 200 °C | 392 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
| Dielectric Constant | 4.12 <br>@Frequency 100000 Hz |
4.12 <br>@Frequency 100000 Hz |
|
| 4.16 <br>@Frequency 100 Hz |
4.16 <br>@Frequency 100 Hz |
||
| 4.8 <br>@Frequency 1.00e+6 Hz |
4.8 <br>@Frequency 1.00e+6 Hz |
||
| Dielectric Strength | 13.0 kV/mm | 329 kV/in | |
| Dissipation Factor | 0.00325 <br>@Frequency 100000 Hz |
0.00325 <br>@Frequency 100000 Hz |
|
| 0.00807 <br>@Frequency 100 Hz |
0.00807 <br>@Frequency 100 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 7200 min <br>@Temperature 22.0 °C |
120 hour <br>@Temperature 71.6 °F |
|
| Shelf Life | 12.0 Month | 12.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | white | |
| Hydrophobic | yes | |
| Self Leveling | yes | |
| Water Resistant | yes | |
| Working Time (min) | <4 |