| Category | Polymer , Adhesive , Thermoset , Silicone |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Dow Corning SE 1880.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.970 g/cc @Temperature 25.0 °C |
0.970 g/cc @Temperature 77.0 °F |
|
| Viscosity | 800 cP | 800 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 85 | 85 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 200 °C | 392 °F | |
| Minimum Service Temperature, Air | -80.0 °C | -112 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.75 @Frequency 1.00e+6 Hz |
2.75 @Frequency 1.00e+6 Hz |
|
| Dielectric Strength | 20.0 kV/mm | 508 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 30.0 min @Temperature 150 °C |
0.500 hour @Temperature 302 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | clear | |
| Color | blue | |
| Flowable | yes | |
| Gel Hardness (Grams/Penetration) | 65 | |
| Hydrophobic | yes | |
| Self Leveling | yes | |
| Water Resistant | yes |