Dow Corning MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, MEDIUM

Category Fluid , Lubricant , Silicone Base
Manufacturer Dow Corning
Trade Name MOLYKOTE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Dow Corning MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, MEDIUM.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Phenyl-methyl silicone grease for low to high temperaturesInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc

@Temperature 25.0 °C
1.05 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 112.1 kg
247.2 lb (mass)
Penetration P(60), 1/10 mm 280
280
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Dropping Point 220 °C
428 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Color white
NLGI Number 2
Thickening System lithium soap