Material Notes:
OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended for use in injection molded applications requiring high impact resistance and good stiffness. The excellent moldability of this product enables short cycle times. It is particularly suited for industrial container, material handling, consumer products, and automotive applications.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3310 psi
ASTM D638
Elongation at Yield 4.5 %
4.5 %
ASTM D638
Flexural Modulus, 1% Secant 1210 MPa
175000 psi
ASTM D790A
Izod Impact, Notched 0.747 J/cm

@Temperature -20.0 °C
1.40 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.854 J/cm

@Temperature 0.000 °C
1.60 ft-lb/in

@Temperature 32.0 °F
ASTM D256A
1.87 J/cm

@Temperature 23.0 °C
3.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
Unannealed; ASTM D648