Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow AFFINITY™ SM 8250 Polyolefin Plastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ SM 8250 Polyolefin Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flexibility, excellent low temperature impact properties and allows the use of hot runner molds to enhance production automation. Its low specific gravity can help control resin and production costs, while reducing the weight of end products.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.885 g/cc
0.0320 lb/in³
Melt Flow 30 g/10 min

@Load 2.16 kg
30 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Tensile Strength, Yield 2.50 MPa
363 psi
Elongation at Break >= 1000 %
>= 1000 %
Modulus of Elasticity 0.0372 GPa
5.40 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.0400 GPa
5.80 ksi
Thermal Properties Metric English Comments
Vicat Softening Point 51.0 °C
124 °F
Users viewing this material also viewed the following: