Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 6.74e-8 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.00000977 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0002943 - 0.0004905 GPa

@Temperature 1000 °C,
Time 10800 sec
0.04269 - 0.07114 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 0.686 - 0.883 MPa

@Temperature 1000 °C,
Time 10800 sec
99.6 - 128 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
1.47 - 1.96 MPa

@Temperature 110 °C,
Time 86400 sec
213 - 284 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.116 - 0.174 W/m-K

@Temperature 540 °C
0.806 - 1.21 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.116 - 0.174 W/m-K

@Temperature 800 °C
0.806 - 1.21 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
limited
Shrinkage -2.00 - -1.50 %

@Temperature 1000 °C,
Time 10800 sec
-2.00 - -1.50 %

@Temperature 1830 °F,
Time 3.00 hour
-0.300 - -0.200 %

@Temperature 110 °C,
Time 86400 sec
-0.300 - -0.200 %

@Temperature 230 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Installation Method Gunning, Casting(UOP)
Main Applications Petrochemical plant Heater, Boiler
Material Required for Estimating (kg/?) 450-550
Water Required for Casting(%) 100