Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers FOMBLIN® W500 PFPE Lubricant

Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® W500 PFPE Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
ASTM D891
Viscosity Measurement 209
209
Viscosity Index; ASTM D2270
Kinematic Viscosity 543 cSt

@Temperature 20.0 °C
543 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 208 cSt
208 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 34 cSt
34 cSt
ASTM D445
Molecular Weight 7200 g/mol
7200 g/mol
Evaporation Loss 0.90 %
0.90 %
22 hrs. at 204°C; ASTM 2595
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 114 kg
251 lb (mass)
Mean Hertz Load; IP 239
562 kg
1240 lb (mass)
Init. Seiz. Load; IP 239
631 kg
1390 lb (mass)
Welding Load; IP 239
Four Ball Wear 0.900 mm
0.0354 in
Avg. scar diameter; ASTM D4172
Thermal Properties Metric English Comments
Pour Point -46.0 °C
-50.8 °F
ASTM D97