Dielectric Polymers NT-2822 Ultra Tack Tape  (discontinued **)

Category Polymer , Adhesive , Tape , Thermoset , Polyester, TS , Silicone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dielectric Polymers NT-2822 Ultra Tack Tape  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film at zero wet out time. For applications where instant adhesion is critical.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Adhesive
50.8 microns
2.00 mil
Backing
Mechanical Properties Metric English Comments
Elongation at Break 90 %
90 %
Peel Strength 0.5478 kN/m
3.125 pli
Adhesion
8.77 kN/m
50.0 pli
Tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
>= 260 °C
>= 500 °F
Shear Adhesive Failure (polyester failure)
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Burgundy