Dielectric Polymers NT-100APS General Purpose Laminating Adhesive  (discontinued **)

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dielectric Polymers NT-100APS General Purpose Laminating Adhesive  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Acrylic adhesive with moisture stable PE coated kraft (60#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panels and decorative trim. For kiss cut applications and bonding a wide variety of substrates.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Adhesive
102 microns
4.00 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.614 kN/m
3.50 pli
180° peel, PET/s.s.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 116 °C
240 °F
Shear Adhesive Failure (cohesive failure)
121 °C
250 °F
Continuous
204 °C
400 °F
Intermittent
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Continuous